2343 Hot Work Tool Steel
Minimum Order Quantity | 200 Kilogram |
Application | Automobile Industry |
Soft annealing Degree C | 750 - 800 |
Hardening Degree C | 1000 -1030 |
Hardness HB | max 230 |
Cooling | Furnace |
Stress relief annealing Degree C | approx 600 - 650 |
We are offering 2343 Hot Work Tool Steel to our clients. It is an all inclusive hot work tool steel with hot rigidity and durability. Good thermal conductivity and invulnerability to hot cracking and can be water cooled to a constrained degree. Utilized for ejector pins, apparatus holders and shrink fit chucks
2343 Hot Work Tool Steel Properties
Hot work tool steel with Chromium 5% has high strength and toughness, best thermal physical phenomenon and in susceptibility to hot cracking. This provides the essential necessities for long tool life in die-casting , Press Forging extrusion processes etc.
2343 Hot Work Tool Steel Physical Properties
Coefficient of thermal expansion °C | 20-100 | 20-200 | 20-300 | 20-400 | 20-500 | 20-600 | 20-700 |
10-6 m/(m*K) | 11.7 | 12.3 | 12.5 | 12.7 | 12.75 | 12.9 | 12.9 |
Thermal Conductivity °C | 20 | 350 | 700 |
W/(m*K)Annealed | 29.8 | 30.0 | 33.5 |
W/(m*K)Quenched & Tempered | 26.7 | 27.4 | 30.4 |
Besides applications typical for the area of hot-work steels, this grade is especially used for ejector pins, tool holders, bridge kind tools, liner holders, Forging Dies, Hot work punches, and shrink work chucks.
Heat Treatment
Soft annealing °C | Cooling | Hardness HB |
---|---|---|
750 – 800 | Furnace | max. 230 |
Stress-relief annealing °C | Cooling |
---|---|
approx. 600 – 650 | Furnace |
Hardening °C | Quenching | Hardness after quenching HRC |
---|---|---|
1000 – 1030 | Air ,oil or saltbath, 500 – 550 °C | 54 |
Tempering °C | 100 | 200 | 300 | 400 | 500 | 550 | 600 | 650 | 700 |
HRC | 52 | 52 | 52 | 52 | 54 | 53 | 48 | 37 | 31 |