Product details
| Minimum Order Quantity | 200 Kg |
| Coefficient of thermal expansion at Degree C | 20-500 Deg C |
| Cooling | Furnace |
| Hardness HB | Max 235 |
| Soft annealing Degree C | 710 - 740 Deg C |
| Thermal Conductivity at Degree C | 20-700 Deg C |
| Thickness | 20 to 400 mm |
| Width | 40 to 700 mm |
| Application | Automobile Industry |
Physical Properties:
| Coefficient of Thermal Expansion at C | 10 m / (m*K) |
| 20-100 | 11.2 |
| 20-200 | 12.8 |
| 20-300 | 13.5 |
| 20-400 | 13.7 |
| 20-500 | 14.3 |
| 20-600 | 14.7 |
| 20-700 | 14.9 |
| Thermal Conductivity at C | W / (m*K) |
| 20 | 35 |
| 350 | 34 |
| 700 | 33 |
Heat Treatment:
| Soft Annealing C | 710-740 |
| Cooling | Furnace |
| Hardness HB | max. 235 |
| Hardening C | 840-870 |
| Quenching | Polymer or Oil |
| Hardness after quenching HRC | 51 |
| TemperingC after quenching | 100 | 200 | 300 | 400 | 500 | 600 | 700 |
| HRC | 51.5 | 50.2 | 48 | 46.2 | 43 | 39 | 29 |